抄録
Fracture and small crack behavior in the very high cycle domain of 10 9 cycles were investigated with a nickel-based superalloy under ultrasonic fatigue in ambient air at room temperature. The influence of ultrasonic frequency is examined by comparing the results with those in conventional low frequency fatigue. It is found that fatigue strength increases as frequency is raised up to 19.5 kHz and the most of fatigue life is consumed in nucleating and propagating small cracks up to 100 μm. Transition of fracture mode from transgranular ductile fracture to cleavage-dominated fracture occurs beyond a critical stress intensity factor range of approximately 21MPam, leading to the catastrophic failure under ultrasonic fatigue.
| 本文言語 | 英語 |
|---|---|
| ページ(範囲) | 1227-1232 |
| ページ数 | 6 |
| ジャーナル | International Journal of Fatigue |
| 巻 | 27 |
| 号 | 10-12 |
| DOI | |
| 出版ステータス | 出版済み - 10月 2005 |
| 外部発表 | はい |
| イベント | Fatigue Damage of Structural Materials V - 継続期間: 9月 19 2004 → 9月 24 2004 |
!!!All Science Journal Classification (ASJC) codes
- モデリングとシミュレーション
- 材料科学一般
- 材料力学
- 機械工学
- 産業および生産工学
フィンガープリント
「Small crack behavior and fracture of nickel-based superalloy under ultrasonic fatigue」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。引用スタイル
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS