F82H is a primary candidate of structural material and coolant pipe material in a blanket of a fusion reactor. Understanding tritium permeation behavior through F82H is important. In a normal operation of a fusion reactor, the temperature of F82H will be controlled below 550 °C because it is considered that F82H can be used up to 30,000 hours at 550 °C. However, it is necessary to assume the situation where F82H is heated over 550 °C in a severe accident. In this study, hydrogen permeation behavior through F82H was investigated in the temperature range from 500 °C to 800 °C. In some cases, water vapor was added in a sample gas to investigate an effect of water vapor on hydrogen permeation. The permeability of hydrogen in the temperature range from 500 °C to 700 °C agreed well with the permeability reported by E. Serra et al. The degradation of the permeability by water vapor was not observed. After the hydrogen permeation reached in a steady state at 700 °C, the F82H sample was heated to 800 °C. The permeability of hydrogen through F82H sample which was once heated up to 800 °C was lower than that of the original one.
| 本文言語 | 英語 |
|---|---|
| ページ(範囲) | 467-470 |
| ページ数 | 4 |
| ジャーナル | Fusion Science and Technology |
| 巻 | 67 |
| 号 | 2 |
| DOI | |
| 出版ステータス | 出版済み - 3月 1 2015 |
!!!All Science Journal Classification (ASJC) codes
- 土木構造工学
- 核物理学および高エネルギー物理学
- 原子力エネルギーおよび原子力工学
- 材料科学一般
- 機械工学
フィンガープリント
「Hydrogen permeation behavior through F82H at high temperature」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。引用スタイル
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS