抄録
In order to investigate the fracture mechanism in fatigue of Ni-base Superalloy at elevated temperatures, rotating bending fatigue tests were carried out for Inconel 718 at 500°C and 600°C up to 108 cycles. At both temperatures, fracture occurred from a subsurface of the specimen in long life region, though the origin of fracture was the specimen surface in short life region. Consequently, S-N curves showed a two-step shape in elevated temperature tests. Although a surface crack was observed similar to the result at room temperature even in long life region at elevated temperatures, the surface crack stopped propagating. In this case, interganular cracks were observed at an origin of subsurface fracture. The subsurface damage was initiated at the early stage of fatigue life.
| 本文言語 | 英語 |
|---|---|
| ページ(範囲) | 1226-1233 |
| ページ数 | 8 |
| ジャーナル | Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A |
| 巻 | 71 |
| 号 | 9 |
| DOI | |
| 出版ステータス | 出版済み - 9月 2005 |
| 外部発表 | はい |
!!!All Science Journal Classification (ASJC) codes
- 材料科学一般
- 材料力学
- 機械工学
フィンガープリント
「Fracture mechanism in fatigue of Ni-base superalloy Inconel 718 at elevated temperatures」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。引用スタイル
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS