抄録
Porous β-tricalcium phosphate (β-TCP) has attracted attention as an artificial bone substitute. α-TCP foam that mimics the fully interconnected porous structure of the cancellous bone can be fabricated by a ceramics foam method, which requires sintering at high temperature. However, β-TCP foam could not be fabricated by the ceramics foam method since the sintering temperature required is above the αβ transition temperature. To fabricate the β-TCP foam that mimics the fully interconnected porous structure of cancellous bone, magnesium oxide (MgO) is added as a phase stabilizer. β-TCP foam was obtained when at least 3 mol% MgO was added. Lattice parameter analysis revealed that the MgO as a β-phase stabilizer was incorporated into the lattice of the TCP structure. The porosity of the β-TCP foam containing 3 mol% MgO was 92%, and the compressive strength was approximately 32 kPa. Despite the observed smooth surface and lower porosity of β-TCP foam compared to α-TCP foam, no improvement on the compressive strength of β-TCP foam occurred even by the addition of 3 mol% or more of MgO. Formation of micro-cracks could be one the reasons. These micro-cracks were formed by contraction as a result from growth of adjacent grains.
| 本文言語 | 英語 |
|---|---|
| ページ(範囲) | 14245-14250 |
| ページ数 | 6 |
| ジャーナル | Ceramics International |
| 巻 | 41 |
| 号 | 10 |
| DOI | |
| 出版ステータス | 出版済み - 5月 7 2015 |
!!!All Science Journal Classification (ASJC) codes
- 電子材料、光学材料、および磁性材料
- セラミックおよび複合材料
- プロセス化学およびプロセス工学
- 表面、皮膜および薄膜
- 材料化学
フィンガープリント
「Fabrication of β-TCP foam: Effects of magnesium oxide as phase stabilizer on its properties」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。引用スタイル
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS