TY - JOUR
T1 - Experimental investigation of tritium release from LiAlO2 and absorption into Zr
AU - Kobayashi, Seiyo
AU - Katayama, Kazunari
AU - Isogawa, Hiroki
AU - Matsuura, Hideaki
AU - Akashi, Kenta
AU - Iinuma, Yuto
N1 - Publisher Copyright:
© 2025
PY - 2026/1
Y1 - 2026/1
N2 - Tritium (T) production using a high-temperature gas-cooled reactor (HTGR) has been proposed to arrange initial T inventory for nuclear fusion reactors. For the establishment of this method, the behavior of T in a Li-loading rod (Li-rod), which contains LiAlO2 and zirconium (Zr), needs to be understood. In this study, a powdered LiAlO2 sample was heated in H2 containing Ar gas flow to observe water formation reaction. Then, a powdered Zr sample was heated in humid Ar gas flow to investigate the temperature dependence of H2O reduction rate on the Zr. Finally, a Zr-mixed LiAlO2 sample, which had been neutron-irradiated in the Kyoto University Research Reactor (KUR), was preheated at 700 °C in a sealed quartz tube, and then heated in Ar gas flow to observe the release behavior of T from the sample. Released gaseous T (HT, T2) and tritiated water vapor (HTO, T2O) were separately collected using a pair of bubblers installed upstream and downstream of a copper oxide (CuO) bed, and the tritium concentration in each bubbler was measured using a liquid scintillation counter. Based on the results, it is suggested that LiAlO2 should be in advance heated in reduction atmosphere to remove adsorbed water and unstable oxygen to suppress the release of T in chemical form of HTO, and Li-rod should be operated at higher temperatures over 700 °C to decrease the mass transfer resistance by an oxide layer on Zr.
AB - Tritium (T) production using a high-temperature gas-cooled reactor (HTGR) has been proposed to arrange initial T inventory for nuclear fusion reactors. For the establishment of this method, the behavior of T in a Li-loading rod (Li-rod), which contains LiAlO2 and zirconium (Zr), needs to be understood. In this study, a powdered LiAlO2 sample was heated in H2 containing Ar gas flow to observe water formation reaction. Then, a powdered Zr sample was heated in humid Ar gas flow to investigate the temperature dependence of H2O reduction rate on the Zr. Finally, a Zr-mixed LiAlO2 sample, which had been neutron-irradiated in the Kyoto University Research Reactor (KUR), was preheated at 700 °C in a sealed quartz tube, and then heated in Ar gas flow to observe the release behavior of T from the sample. Released gaseous T (HT, T2) and tritiated water vapor (HTO, T2O) were separately collected using a pair of bubblers installed upstream and downstream of a copper oxide (CuO) bed, and the tritium concentration in each bubbler was measured using a liquid scintillation counter. Based on the results, it is suggested that LiAlO2 should be in advance heated in reduction atmosphere to remove adsorbed water and unstable oxygen to suppress the release of T in chemical form of HTO, and Li-rod should be operated at higher temperatures over 700 °C to decrease the mass transfer resistance by an oxide layer on Zr.
KW - High-temperature gas-cooled reactor (HTGR)
KW - Initial tritium inventory
KW - Lithium aluminate (LiAlO)
KW - Nuclear fusion reactor
KW - Tritium
KW - Zirconium (Zr)
UR - https://www.scopus.com/pages/publications/105017509047
UR - https://www.scopus.com/pages/publications/105017509047#tab=citedBy
U2 - 10.1016/j.fusengdes.2025.115471
DO - 10.1016/j.fusengdes.2025.115471
M3 - Article
AN - SCOPUS:105017509047
SN - 0920-3796
VL - 222
JO - Fusion Engineering and Design
JF - Fusion Engineering and Design
M1 - 115471
ER -