The acicular ferrite (AF) formation behaviors of submerged arc weld metals with various Al/O ratios and Mn contents were investigated. The nucleation sites of AF consisted of inclusions surrounded by a TiO layer. The Al/O ratio affected the number of inclusions that acted as AF nucleation sites. At high Al/O ratios, the number of inclusions was low and the microstructure was coarse. We considered that the formation of AF was promoted by the presence of the TiO layer via two mechanisms: Good lattice matching with ferrite and formation of a Mn-depleted zone owing to the absorption of Mn. The Baker-Nutting orientation relationship between TiO and AF was observed. Moreover, we determined that Mn-depleted zones were formed around the inclusions surrounded by TiO. The Mn content of weld metals affected the formation of AF via the formation of Mn-depleted zones. When the Mn content of the weld metals was high, Mn-depleted zones were formed.

本文言語英語
ページ(範囲)1614-1622
ページ数9
ジャーナルisij international
61
5
DOI
出版ステータス出版済み - 2021
外部発表はい

!!!All Science Journal Classification (ASJC) codes

  • 材料力学
  • 機械工学
  • 金属および合金
  • 材料化学

フィンガープリント

「Effects of Mn and Al on acicular ferrite formation in SAW weld metal」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル