TY - JOUR
T1 - Effect of laser annealing using high repetition rate pulsed laser on optical properties of phosphorus-ion-implanted ZnO nanorods
AU - Shimogaki, Tetsuya
AU - Ofuji, Taihei
AU - Tetsuyama, Norihiro
AU - Okazaki, Kota
AU - Higashihata, Mitsuhiro
AU - Nakamura, Daisuke
AU - Ikenoue, Hiroshi
AU - Asano, Tanemasa
AU - Okada, Tatsuo
N1 - Funding Information:
The authors would like to thank Mr. Takayuki Takao and Mr. Yosuke Watanabe of the Department of Gigaphoton Next GLP for their support in the experiment. This work was supported in part by the Program under Special Coordination Funds for Promoting Science and Technology from the Japan Science and Technology Agency (JST) and a Grant-in-Aid for Scientific Research from the Japan Society for the Promotion of Science (JSPS, No. 24656053).
PY - 2014/2
Y1 - 2014/2
N2 - The effect of high repetition rate pulsed laser annealing with a KrF excimer laser on the optical properties of phosphorus-ion-implanted zinc oxide nanorods has been investigated. The recovery levels of phosphorus-ion-implanted zinc oxide nanorods have been measured by photoluminescence spectra and cathode luminescence images. Cathode luminescence disappeared over 300 nm below the surface due to the damage caused by ion implantation with an acceleration voltage of 25 kV. When the annealing was performed at a low repetition rate of the KrF excimer laser, cathode luminescence was recovered only in a shallow area below the surface. The depth of the annealed area was increased along with the repetition rate of the annealing laser. By optimizing the annealing conditions such as the repetition rate, the irradiation fluence and so on, we have succeeded in annealing the whole damaged area of over 300 nm in depth and in observing cathode luminescence. Thus, the effectiveness of high repetition rate pulsed laser annealing on phosphorus-ion-implanted zinc oxide nanorods was demonstrated.
AB - The effect of high repetition rate pulsed laser annealing with a KrF excimer laser on the optical properties of phosphorus-ion-implanted zinc oxide nanorods has been investigated. The recovery levels of phosphorus-ion-implanted zinc oxide nanorods have been measured by photoluminescence spectra and cathode luminescence images. Cathode luminescence disappeared over 300 nm below the surface due to the damage caused by ion implantation with an acceleration voltage of 25 kV. When the annealing was performed at a low repetition rate of the KrF excimer laser, cathode luminescence was recovered only in a shallow area below the surface. The depth of the annealed area was increased along with the repetition rate of the annealing laser. By optimizing the annealing conditions such as the repetition rate, the irradiation fluence and so on, we have succeeded in annealing the whole damaged area of over 300 nm in depth and in observing cathode luminescence. Thus, the effectiveness of high repetition rate pulsed laser annealing on phosphorus-ion-implanted zinc oxide nanorods was demonstrated.
UR - http://www.scopus.com/inward/record.url?scp=84893751626&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=84893751626&partnerID=8YFLogxK
U2 - 10.1007/s00339-013-7638-y
DO - 10.1007/s00339-013-7638-y
M3 - Article
AN - SCOPUS:84893751626
SN - 0947-8396
VL - 114
SP - 625
EP - 629
JO - Applied Physics A: Materials Science and Processing
JF - Applied Physics A: Materials Science and Processing
IS - 2
ER -