Durability analysis of polymer-coated pristine carbon nanotube-based fuel cell electrocatalysts under non-humidified conditions

    研究成果: ジャーナルへの寄稿 › 学術誌 › 査読

    抄録

    A polymer electrolyte fuel cell (PEFC) that shows high durability at elevated temperature and under non-humidified conditions is strongly demanded for the next generation PEFCs. Here we show the importance of using pristine carbon nanotubes (CNTs) as catalyst supports for fuel cell (FC) durability. For that purpose, two different membrane electrode assemblies (MEAs) using pristine CNTs and commercial carbon black (CB) as carbon supports were coated by polybenzimidazole on which platinum (Pt) nanoparticles were deposited. Notably, the CNT-based MEA exhibited ∼4 times higher durability compared to the CB-based MEA. The ex situ monitoring of the fabricated electrocatalysts before and after the durability testing based on transmission electron microscopy and X-ray diffraction measurements revealed higher structural stability of the CNTs compared to the CB in their MEAs. The pristine structure of the CNTs has been revealed to be very important for the high PEFC durability. This is the first report that shows the durability of the pristine CNT-based PEFC at high operating temperature and under non-humidified conditions, which are the targets of the next generation PEFCs with very high performance.

    本文言語英語
    ページ(範囲)19053-19059
    ページ数7
    ジャーナルJournal of Materials Chemistry A
    巻2
    号44
    DOI
    出版ステータス出版済み - 11月 28 2014

    UN SDG

    この成果は、次の持続可能な開発目標に貢献しています

    1. SDG 7 - エネルギーをみんなに そしてクリーンに
      SDG 7 エネルギーをみんなに そしてクリーンに

    !!!All Science Journal Classification (ASJC) codes

    • 化学一般
    • 再生可能エネルギー、持続可能性、環境
    • 材料科学一般

    フィンガープリント

    「Durability analysis of polymer-coated pristine carbon nanotube-based fuel cell electrocatalysts under non-humidified conditions」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

    引用スタイル