Characterization of Metal/Glass Interfaces in Bioactive Glass Coatings on Ti-6Al-4V and Co-Cr Alloys

E. Saiz, S. Lopez-Esteban, S. Fujino, T. Oku, K. Suganuma, A. P. Tomsia

    研究成果: 書籍/レポート タイプへの寄稿

    4 被引用数 (Scopus)

    抄録

    This chapter reveals that coating metallic-based implants with bioactive materials promotes joining between the prostheses and the bone, as well as increases long-term implant stability. The interface between different alloys and bioactive silicate glass coatings, prepared using a simple enameling technique, is analyzed at the nano level. Transmission electron microscopy and associated chemical analysis of the glass/alloy interface show the formation of thin Ti5Si3 or CrOx reaction layers. These nano structured interfaces facilitate the formation of a stable joint between the glass coating and the alloys. Nowadays, biomaterials such as Ti or Co-Cr alloys are widely used in orthopedic and dental implants. However, their long-term effectiveness needs improvement. In particular, metallic implants have a variety of shortcomings related to their affixation, and in many cases, failures are caused by poor adhesion of the implant to the tissue or bone. A commonly used strategy to improve osseointegration is to coat the alloys with a bioactive material that will accelerate the stabilization of the implant and extend its duration.

    本文言語英語
    ホスト出版物のタイトルNano and Microstructural Design of Advanced Materials
    ホスト出版物のサブタイトルA Commemorative Volume on Professor G. Thomas' Seventieth Birthday
    出版社Elsevier Inc.
    ページ61-67
    ページ数7
    ISBN(電子版)9780080537238
    ISBN(印刷版)9780080443737
    DOI
    出版ステータス出版済み - 12月 5 2003

    !!!All Science Journal Classification (ASJC) codes

    • 工学(全般)
    • 材料科学(全般)

    フィンガープリント

    「Characterization of Metal/Glass Interfaces in Bioactive Glass Coatings on Ti-6Al-4V and Co-Cr Alloys」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

    引用スタイル