TY - JOUR
T1 - Changes in surface roughness and colour stability of soft denture lining materials caused by denture cleansers
AU - Jin, C.
AU - Nikawa, H.
AU - Makihira, S.
AU - Hamada, T.
AU - Furukawa, M.
AU - Murata, H.
PY - 2003/2/1
Y1 - 2003/2/1
N2 - Soft denture lining materials were immersed into solutions of denture cleansers for 8 h at room temperature, and immersed into distilled water for the remainder of the 24-h period at 37°C. Surface roughness of the soft denture lining materials was measured by contact type surface roughness instrument. For the colour stability test, soft denture lining materials were immersed in the denture cleansers as described above for 180 days. Finally, the colour changes of each material were quantitatively measured by a photometrical instrument to obtain the colour differences between newly processed specimen and immersed specimens (P < 0.01). An autopolymerizing silicone material, Evatouch, exhibited severe changes in surface roughness by all denture cleanser, and the generic material GC Denture Relining showed the minimal changes. Severe colour changes were also observed with some liner and cleanser combinations (P < 0.01). Except for Evatouth, the four silicone soft liners were more stable in surface roughness and in colour change than the two acrylic soft liners. One autopolymerizing silicone (GC denture relining) and one heat curing silicone (Molloplast B) demonstrated the best stability.
AB - Soft denture lining materials were immersed into solutions of denture cleansers for 8 h at room temperature, and immersed into distilled water for the remainder of the 24-h period at 37°C. Surface roughness of the soft denture lining materials was measured by contact type surface roughness instrument. For the colour stability test, soft denture lining materials were immersed in the denture cleansers as described above for 180 days. Finally, the colour changes of each material were quantitatively measured by a photometrical instrument to obtain the colour differences between newly processed specimen and immersed specimens (P < 0.01). An autopolymerizing silicone material, Evatouch, exhibited severe changes in surface roughness by all denture cleanser, and the generic material GC Denture Relining showed the minimal changes. Severe colour changes were also observed with some liner and cleanser combinations (P < 0.01). Except for Evatouth, the four silicone soft liners were more stable in surface roughness and in colour change than the two acrylic soft liners. One autopolymerizing silicone (GC denture relining) and one heat curing silicone (Molloplast B) demonstrated the best stability.
UR - http://www.scopus.com/inward/record.url?scp=0037317989&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=0037317989&partnerID=8YFLogxK
U2 - 10.1046/j.1365-2842.2003.01014.x
DO - 10.1046/j.1365-2842.2003.01014.x
M3 - Article
C2 - 12535137
AN - SCOPUS:0037317989
SN - 0305-182X
VL - 30
SP - 125
EP - 130
JO - Journal of oral rehabilitation
JF - Journal of oral rehabilitation
IS - 2
ER -