@inproceedings{7180077c1a9f4817b6d2bfd40594d0a6,
title = "4D characterization of the stress corrosion cracking behavior in Al-10Mg aluminium alloy via synchrotron X-ray tomography",
abstract = "Stress corrosion cracking (SCC) behavior of Al-10Mg aluminium alloys is studied with the help of the high resolution X-ray tomography in the present research. The SCC-induced crack is formed from the corrosion pit near the surface, and gradually propagates and coalescence with the voids due to the fracture of β phase ahead of the crack tip at low applied strain levels. In addition, hydrogen concentration in the ligament between the SCC-induced crack tip and voids accelerates the propagation of the crack, indicating that hydrogen concentration and partitioning among various trap sites dominates the SCC and entire fracture of Al-10Mg aluminium alloys.",
author = "Dongsheng Fu and Hiroyuki Toda and Hang Su and Kyosuke Hirayama and Kentaro Uesugi and Akihisa Takeuchi",
note = "Funding Information: The authors gratefully acknowledge the support from SPing-8. The synchrotron radiation experiments were performed through proposal No. 2016A1199 and 2016B1081 with the approval of JASRI. The support provided by the Light Metal Educational Foundation to the author H.T is also gratefully acknowledged. Publisher Copyright: {\textcopyright} 2019 by the International Society of Offshore and Polar Engineers (ISOPE).; 29th International Ocean and Polar Engineering Conference, ISOPE 2019 ; Conference date: 16-06-2019 Through 21-06-2019",
year = "2019",
language = "English",
isbn = "9781880653852",
series = "Proceedings of the International Offshore and Polar Engineering Conference",
publisher = "International Society of Offshore and Polar Engineers",
pages = "4199--4203",
editor = "Chung, {Jin S.} and Akselsen, {Odd M.} and HyunWoo Jin and Hiroyasu Kawai and Yongwon Lee and Dmitri Matskevitch and {Ho Van}, Suak and Decheng Wan and Wang, {Alan M.} and Satoru Yamaguchi",
booktitle = "Proceedings of the 29th International Ocean and Polar Engineering Conference, ISOPE 2019",
address = "United States",
}