Abstract
A nanoporous FePt alloy has been fabricated by dealloying a melt-spun Fe60Pt20B20 alloy composed of nanoscale amorphous and face-centered-cubic FePt (fcc-FePt) phases in H2SO4 aqueous solution. The nanoporous alloy consists of single fcc-FePt phase with an Fe/Pt atomic ratio of about 55.3/44.7, and possesses a uniform interpenetrating ligament-channel structure with average ligament and pore sizes of 27 nm and 12 nm, respectively. The nanoporous fcc-FePt alloy shows soft magnetic characteristics with a saturation magnetization of 37.9 emu/g and better electrocatalytic activity for methanol oxidation than commercial Pt/C in acidic environment. The phase transformation from disordered fcc-FePt into ordered face-centered-tetragonal FePt (L10-FePt) in the nanoporous alloy has been realized after annealing at 823–943 K for 600 s. The volume fraction of the L10-FePt phase in the alloy increases with the rise of annealing temperature, which results in the enhancements of coercivity and saturation magnetization from 0.14 kOe and 38.5 emu/g to 8.42 kOe and 51.4 emu/g, respectively. The ligament size of the samples is increased after annealing.
Original language | English |
---|---|
Pages (from-to) | 128-133 |
Number of pages | 6 |
Journal | Journal of Materials Science and Technology |
Volume | 36 |
DOIs | |
Publication status | Published - Jan 1 2020 |
Externally published | Yes |
All Science Journal Classification (ASJC) codes
- Ceramics and Composites
- Mechanics of Materials
- Mechanical Engineering
- Polymers and Plastics
- Metals and Alloys
- Materials Chemistry