The organic-organic self-assembly method with Resorcinol (R)/Formaldehyde (F) and Pluronic F127 has been employed to synthesize mesoporous carbon (MC). The pore diameter of the MC has been tuned from 7 to 12.5 nm by changing the molar ratio of carbon sources to surfactant and polymerization time.