Abstract
Interconnected macroporous calcium phosphate has attracted attention as an artificial bone substitute as well as a scaffold for tissue engineering. In this investigation, a setting reaction between α-tricalcium phosphate (α-TCP) spheres and an acidic calcium phosphate solution (0.2 mol/L monocalcium phosphate monohydrate – 0.1 mol/L phosphoric acid) was studied to assess the feasibility of fabricating fully interconnected macroporous calcium phosphate. When 1.3 mm-diameter α-TCP spheres were exposed to an acidic calcium phosphate solution, brushite (dicalcium phosphate dihydrate) was formed on the surface of the α-TCP spheres. The precipitated brushite crystals interlocked with one another and bridged the α-TCP spheres, resulting in a 10 min setting reaction at 37 °C that produced fully interconnected macroporous calcium phosphate. The resultant calcium phosphate macroporous structure had a porosity of 49.7±2.5% and an average pore size of 312±160 μm.
| Original language | English |
|---|---|
| Pages (from-to) | 13525-13531 |
| Number of pages | 7 |
| Journal | Ceramics International |
| Volume | 41 |
| Issue number | 10 |
| DOIs | |
| Publication status | Published - Dec 2015 |
All Science Journal Classification (ASJC) codes
- Electronic, Optical and Magnetic Materials
- Ceramics and Composites
- Process Chemistry and Technology
- Surfaces, Coatings and Films
- Materials Chemistry
Fingerprint
Dive into the research topics of 'Setting reaction of α-TCP spheres and an acidic calcium phosphate solution for the fabrication of fully interconnected macroporous calcium phosphate'. Together they form a unique fingerprint.Cite this