Pitting corrosion resistance of anodized aluminum-copper alloy processed by severe plastic deformation

In Joon Son, Hiroaki Nakano, Satoshi Oue, Shigeo Kobayashi, Hisaaki Fukushima, Zenji Horita

    Research output: Contribution to journalArticlepeer-review

    4 Citations (Scopus)

    Abstract

    The effect of equal-channel angular pressing (ECAP) on the pitting corrosion resistance of anodized Al-Cu alloy was investigated by electrochemical techniques in a solution containing 0.2 mol/L of AlCl3 and also by surface analysis. The time required before initiating pitting corrosion of anodized Al-Cu alloy was longer with ECAP than without, indicating improvement in the pitting corrosion resistance by application of ECAP. Second phase precipitates were present in Al-Cu alloy matrix and the size of these precipitates was greatly decreased by application of ECAP. The precipitates composed of Si and Al-Cu-Si-Fe-Mn were not oxidized during anodization, and the anodic oxide film were absent at the boundary between the normal oxide films and these impurity precipitates. The pitting corrosion of anodized Al-Cu alloy occurred preferentially around these precipitates, the improvement of pitting corrosion resistance of anodized Al-Cu alloy by ECAP appears to be attributable to a decrease in the size of precipitates, which act as origins of pitting corrosion.

    Original languageEnglish
    Pages (from-to)353-359
    Number of pages7
    JournalNippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals
    Volume72
    Issue number5
    DOIs
    Publication statusPublished - May 2008

    All Science Journal Classification (ASJC) codes

    • Condensed Matter Physics
    • Mechanics of Materials
    • Metals and Alloys
    • Materials Chemistry

    Fingerprint

    Dive into the research topics of 'Pitting corrosion resistance of anodized aluminum-copper alloy processed by severe plastic deformation'. Together they form a unique fingerprint.

    Cite this