Abstract
The phase transformations of Mg 1.4Pr 0.6Ni 4 and Mg 1.0Pr 1.0Ni 4 during hydrogenation and dehydrogenation were investigated using in situ X-ray diffraction (XRD). Both alloys showed the cubic MgCu 4Sn type structure with space group F4̄3m before hydrogenation. The hydride β-Mg 1.4Pr 0.6Ni 4H ∼3.6 had the same crystal structure as the starting alloy, and its lattice was expanded by 4.3% by hydrogenation. Mg 1.0Pr 1.0Ni 4 was initially transformed to an orthorhombic β-Mg 1.0Pr 1.0Ni 4H ∼4 with space group Pmn2 1. By further hydrogenation, the orthorhombic hydride changed to β-Mg 1.0Pr 1.0Ni 4H ∼6 with a cubic structure with space group F4̄3m. The lattice constant of β-Mg 1.0Pr 1.0Ni 4H ∼6 was 7.6% larger than that of the starting alloy. Through dehydrogenation, all hydride phases returned to the alloy phase without any amorphization or disproportionation.
| Original language | English |
|---|---|
| Pages (from-to) | 1401-1407 |
| Number of pages | 7 |
| Journal | Journal of Physical Chemistry C |
| Volume | 116 |
| Issue number | 1 |
| DOIs | |
| Publication status | Published - Jan 12 2012 |
All Science Journal Classification (ASJC) codes
- Electronic, Optical and Magnetic Materials
- General Energy
- Physical and Theoretical Chemistry
- Surfaces, Coatings and Films
Fingerprint
Dive into the research topics of 'In situ x-ray diffraction study of phase transformation of Mg 2-xPr xNi 4 during hydrogenation and dehydrogenation (x = 0.6 and 1.0)'. Together they form a unique fingerprint.Cite this
- APA
- Standard
- Harvard
- Vancouver
- Author
- BIBTEX
- RIS