Abstract
The authors regret that in the above article we have identified an error on a chemical composition of C in DP steel. This corrigendum is intended to correct the error. In page 402, Line 34 to Line 35 in left paragraph, sentences “A DP steel with a chemical composition of 0.01 C, 0.1 Mn and balance iron in mass %, was prepared.” should be corrected as: “A DP steel with a chemical composition of 0.1 C, 0.1 Mn and balance iron in mass %, was prepared.” The authors would like to apologize for any inconvenience caused.
Original language | English |
---|---|
Pages (from-to) | 441 |
Number of pages | 1 |
Journal | Acta Materialia |
Volume | 133 |
DOIs |
|
Publication status | Published - Jul 2017 |
All Science Journal Classification (ASJC) codes
- Electronic, Optical and Magnetic Materials
- Ceramics and Composites
- Polymers and Plastics
- Metals and Alloys