N2 - An attempt was made to recover the strength of a PIP-processed SiC/SiC composite exposed in air at high temperatures by means of the deoxidization treatment with CO gas. By deoxidation treatment at 1723 and 1823 K for the composite specimen oxidized at 1573 K, the strength of deoxidized specimens became higher by around 4 and 1.5 times than that of oxidized one, respectively.
AB - An attempt was made to recover the strength of a PIP-processed SiC/SiC composite exposed in air at high temperatures by means of the deoxidization treatment with CO gas. By deoxidation treatment at 1723 and 1823 K for the composite specimen oxidized at 1573 K, the strength of deoxidized specimens became higher by around 4 and 1.5 times than that of oxidized one, respectively.
UR - http://www.scopus.com/inward/record.url?scp=28844474921&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=28844474921&partnerID=8YFLogxK
U2 - 10.1163/156855405774984057
DO - 10.1163/156855405774984057
M3 - Article
AN - SCOPUS:28844474921
SN - 0927-6440
VL - 12
SP - 853
EP - 858
JO - Composite Interfaces
JF - Composite Interfaces
IS - 8-9
ER -